  • html
  • text
  • asciidoc
  • rtf
Sintering characteristics of BCSAF cement clinker with added wastes from production of manganese and magnesium metals
School of Materials Science & Engineering, Beifang University of Nationalities, Yinchuan.
Luleå tekniska universitet, Institutionen för samhällsbyggnad och naturresurser, Mineralteknik och metallurgi.
School of Material Science and Engineering, Beifang University for Nationalities Yinchuan, Ningxia.
Department of Ferrous Metallurgy, School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing.
Vise andre og tillknytning
2017 (engelsk)Inngår i: Advances in Cement Research, ISSN 0951-7197, E-ISSN 1751-7605, Vol. 29, nr 6, s. 227-235Artikkel i tidsskrift (Fagfellevurdert) Published
Abstract [en]

The production of belite-calcium sulfoaluminate-ferrite (BCSAF) cement with the addition of industrial wastes as feedstock has been studied for many years. The preparation of clinkers is essential in cement production, in which all raw materials react with each other to generate key phases in cement under some specified conditions. The objective of this study was to investigate the sintering characteristics of BCSAF cement clinkers. Four BCSAF clinkers with different compositions were examined. High-temperature microscopy, quantitative x-ray powder diffraction analysis and scanning electron microscopy were used to analyse sintering features and phase composition. The results show that the use of wastes from the production of manganese and magnesium metals, which were added to the raw materials to make clinker pellets, can significantly reduce the firing temperature of BCSAF clinker. The firing temperatures of clinkers with added wastes were below 1300°C, much lower than the temperature used for conventional Portland cement (1450°C). The ferrite phase was always found to inter-grow with the C4A3S¯">C 4 A 3 S ¯  C4A3S¯ phase or C2AS phase, just like the interstitial phase. The ferrite phase acted as a solid solution during cement sintering. A small quantity of iron oxide can make the clinker more porous, leading to energy savings in subsequent grinding processes.

sted, utgiver, år, opplag, sider
ICE Publishing , 2017. Vol. 29, nr 6, s. 227-235
HSV kategori
Forskningsprogram
Processmetallurgi
Identifikatorer
URN: urn:nbn:se:ltu:diva-63508DOI: 10.1680/jadcr.16.00035ISI: 000401359100001Scopus ID: 2-s2.0-85030786385OAI: oai:DiVA.org:ltu-63508DiVA, id: diva2:1098144
Merknad

Validerad; 2017; Nivå 2; 2017-05-23 (andbra)

Tilgjengelig fra: 2017-05-23 Laget: 2017-05-23 Sist oppdatert: 2018-07-10bibliografisk kontrollert

Open Access i DiVA

Fulltekst mangler i DiVA

Andre lenker

Forlagets fulltekstScopus

Personposter BETA

Yang, Qixing

Søk i DiVA

Av forfatter/redaktør
Yang, Qixing
Av organisasjonen
I samme tidsskrift
Advances in Cement Research

Søk utenfor DiVA

GoogleGoogle Scholar

doi
urn-nbn

Altmetric

doi
urn-nbn
Totalt: 106 treff
RefereraExporteraLink to record
Permanent link

Direct link
Referera
Referensformat
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Annet format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annet språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf