Tribological degradation of MoS2-Ti sputtered coating when exposed to elevated temperatures
Luleå tekniska universitet, Institutionen för teknikvetenskap och matematik, Maskinelement.ORCID-id: 0000-0003-1162-4671
Atatürk University, Faculty of Engineering, Department of Mechanical Engineering, Erzurum.
2010 (engelsk)Inngår i: Tribology - Materials, Surfaces & Interfaces, ISSN 1751-5831, E-ISSN 1751-584X, Vol. 4, nr 3, s. 121-129Artikkel i tidsskrift (Fagfellevurdert) Published
Abstract [en]

The use of solid lubricants is an effective way to control friction and wear in applications where traditional lubricants such as oils and greases cannot be used. MoS2 is a popular solid lubricant which has been widely used in many applications, especially space applications in view of its good performance in vacuum. Recent developments in physical vapour deposition technology have led to the development of sputtered MoS2 films doped with different metals to improve their durability and reduce the detrimental effects of oxidation and humidity on their tribological performance. In this work, a MoS2-Ti coating deposited on a hot forming tool steel substrate has been studied at ambient and elevated temperatures. The objective was to investigate how the friction and durability of the MoS2-Ti coating are affected after exposure to elevated temperatures. The results have shown that low friction values of ∼0·02 were obtained at room temperature and low relative humidity of 25%. An increase in relative humidity to 40% led to an increase in friction by almost 100%. There was a very significant degradation in frictional characteristics as well as durability after the MoS2-Ti coating was exposed to 400°C. The wear of the counter surface also increased when sliding against the MoS2-Ti coating exposed to elevated temperatures. This has been attributed to interaction of the counterbody with hard abrasive molybdenum oxides formed on the MoS2-Ti coating due to exposure to elevated temperatures.

sted, utgiver, år, opplag, sider
2010. Vol. 4, nr 3, s. 121-129
HSV kategori
Forskningsprogram
Maskinelement
Identifikatorer
URN: urn:nbn:se:ltu:diva-4981DOI: 10.1179/175158310X12626998129752ISI: 000444555100004Scopus ID: 2-s2.0-77957563005Lokal ID: 2fec7c30-d2e7-11df-a707-000ea68e967bOAI: oai:DiVA.org:ltu-4981DiVA, id: diva2:977855
Merknad
Godkänd; 2010; 20101008 (jenhar)Tilgjengelig fra: 2016-09-29 Laget: 2016-09-29 Sist oppdatert: 2025-02-14bibliografisk kontrollert

Open Access i DiVA

Fulltekst mangler i DiVA

Andre lenker

Forlagets fulltekstScopus

Person

Hardell, JensPrakash, Braham

Søk i DiVA

Av forfatter/redaktør
Hardell, JensPrakash, Braham
Av organisasjonen
I samme tidsskrift
Tribology - Materials, Surfaces & Interfaces

Søk utenfor DiVA

GoogleGoogle Scholar

doi
urn-nbn

Altmetric

doi
urn-nbn
Totalt: 375 treff
RefereraExporteraLink to record
Permanent link

Direct link
Referera
Referensformat
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Annet format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annet språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf