The heat treated (HT) ThermoD and untreated species were tested for the extreme climate changes. The experimental contained five cycles of soaking in water, freezing and warming. After experimental all samples degraded in colour more or less and some started to crack. ThermoD beech showed the best results. The colour did not change significantly and the material did not crack.