Identification of cracking issues and process improvements through plant monitoring and numerical modelling of secondary cooling during continuous casting of HSLA steels
Luleå University of Technology, Department of Engineering Sciences and Mathematics, Material Science.ORCID iD: 0000-0001-5676-3806
SWERIM. (Raw Materials and Quality)
Luleå University of Technology, Department of Engineering Sciences and Mathematics, Material Science.ORCID iD: 0000-0002-9100-7982
SWERIM. (Raw Materials and Quality)
Show others and affiliations
2020 (English)In: The Iron and Steel Institute of Japan, ISIJ, Vol. 61, no 3, article id ISIJINT-2020-442.R1Article in journal (Refereed) Accepted
Abstract [en]

A holistic approach to diagnose the occurrence of cracking on HSLA steel slabs and propose countermeasures to prevent them is presented. The approach consisted on plant monitoring, including direct temperature measurements in the strand with pyrometers. Extensive characterization was performed via thermo-mechanical tests and microscopy techniques which revealed combination of Widmanstätten ferrite, acicular ferrite and secondary phases that promote embrittlement during casting with a minimum ductility between 700°C-800°C (± 50  ) which is responsible for cracking in this steel. Finally, 1D and 3D numerical models were developed to test possible cooling strategies which proved that reductions in water flowrate can have a positive effect in slab quality by avoiding the low ductility zone. Corrective actions included decreasing cooling to increase the overall temperature of the strand before the straightener to increase the overall temperature. Yet, some slabs still observed the presence of cracks which points at secondary factors such as high tundish temperatures >1530°C producing cracking. Other secondary factors include strong temperature variations up to ± 250 ºC during measurements which would send the strand corners into the low ductility range producing cracking despite having a hot slab centre. Although these optimization strategies are particular to each caster and steel grade, a similar approach could be applied to address secondary cooling issues during continuous casting. The models presented are an ideal toolkit to analyse the influence of product size and operation parameters in combination with plant monitoring and extensive microstructure characterization to improve the quality and productivity of the process.

Place, publisher, year, edition, pages
Japan, 2020. Vol. 61, no 3, article id ISIJINT-2020-442.R1
Keywords [en]
Continuous casting, HSLA steels, plant monitoring, crack susceptibility, cooling curves
National Category
Materials Engineering
Research subject
Engineering Materials
Identifiers
URN: urn:nbn:se:ltu:diva-81108OAI: oai:DiVA.org:ltu-81108DiVA, id: diva2:1475417
Available from: 2020-10-12 Created: 2020-10-12 Last updated: 2023-09-05
In thesis
1. Cracking during Continuous Casting of Steels: Analysis tools and procedures to identify their causes on microalloyed steel slabs
Open this publication in new window or tab >>Cracking during Continuous Casting of Steels: Analysis tools and procedures to identify their causes on microalloyed steel slabs
2020 (English)Doctoral thesis, comprehensive summary (Other academic)
Abstract [en]

Transverse corner cracks are one of the most common but complex defects formed in microalloyed steels during continuous casting (CC). Such cracks are detrimental because it leads to a loss in productivity with a great impact on environment, energy and economics for several steel making companies all over the world. If cracks are detected, a supplementary process has to be applied to remove these cracks (e.g. grinding and scarfing). If cracks cannot be detected due to oxide scales covering the cracks, then they propagate during subsequent processing (e.g. hot rolling), promoting breakouts, which consequently results in material rejection and yield loss.

This thesis focuses on the study of different phenomena occurring during the secondary cooling zone combining the effect of the process parameters together with the material behaviour, which assembles four scientific articles that explains and identifies some of the risks for cracking formation during CC of a HSLA steel slab. This information is key to avoid productivity losses and defect formation in the final cast product. These made possible to address research gaps and better understanding of the steel failure during CC. Additionally, this work proposes the development of strategies for reducing/preventing the formation of cracks during continuous casting of a specific HSLA alloy and caster machine.

Crack susceptibility of the steel was determined through the so called hot ductility method, this made possible to identify the temperature range at which the steel is more susceptible to crack between 700-800 °C. It was found that one of the causes for failure of the steel at high temperatures is the combination of different ferrite morphologies being Widmanstätten ferrite the predominant phase, which is considered unfavourable to toughness and ductility. This temperature range was considered detrimental for cracking formation, which was demonstrated by including real temperature measurements with pyrometers and numerical modelling, that by avoiding the low ductility zone, the quality of the slabs could improve significantly. Outcomes of this work demonstrated that the control of the cooling is beneficial for the process in order to decrease the risk for crack susceptibility of the steel during processing.

Oxide scale formation was considered another important factor that influences the cooling and final quality of steel slabs during CC. The formation of oxide films during cooling of the strand has industrial implications in terms of crack formation and the overall yield of the continuous casting machine since this reduces the cooling efficiency of the strand. Accurate insights in this particular work provides an understanding of oxide scale morphology, type and mechanisms leading to an accurate control of its formation during casting. Some of the findings revealed that oxidation rate and scale thickness is much higher under water vapour than in dry air. The presence of different oxides (i.e. wüstite, magnetite and hematite) change the oxidation behaviour due to micro-mechanical properties that shown higher plasticity for wüstite in comparison to magnetite and hematite. Furthermore, it was demonstrated that the oxide scale not only is influenced by temperature and environmental condition but by the surface of the substrate. These factors are considered one of the reason for uneven cooling during CC process, thus affecting the heat transfer coefficient resulting in undesired surface quality of steel slabs.

Place, publisher, year, edition, pages
Luleå: Luleå University of Technology, 2020. p. 130
Series
Doctoral thesis / Luleå University of Technology 1 jan 1997 → …, ISSN 1402-1544
Keywords
Transverse corner cracks, Continuous Casting, Microalloyes steels, Secondary cooling, Cooling curves, Crack susceptibility
National Category
Metallurgy and Metallic Materials Other Materials Engineering
Research subject
Engineering Materials
Identifiers
urn:nbn:se:ltu:diva-81109 (URN)978-91-7790-677-3 (ISBN)978-91-7790-678-0 (ISBN)
Public defence
2020-11-27, E632, Luleå University of Technology, Luleå, 09:00 (English)
Opponent
Supervisors
Available from: 2020-10-13 Created: 2020-10-12 Last updated: 2023-09-05Bibliographically approved

Open Access in DiVA

No full text in DiVA

Authority records

Pineda Huitron, Rosa MariaVuorinen, Esa

Search in DiVA

By author/editor
Pineda Huitron, Rosa MariaVuorinen, Esa
By organisation
Material Science
Materials Engineering

Search outside of DiVA

GoogleGoogle Scholar

urn-nbn

Altmetric score

urn-nbn
Total: 179 hits
CiteExportLink to record
Permanent link

Direct link
Cite
Citation style
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Other style
More styles
Language
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Other locale
More languages
Output format
  • html
  • text
  • asciidoc
  • rtf