Laser welding, arc welding, and laser-arc hybrid welding can all result in undercut and varying penetration. In some cases, it is technically and commercially viable to reduce undercut at the weld cap and smooth out the weld root profile by defocussing the welding laser and using it to remelt the welded surfaces.