A fractographic study exploring the relationship between the low cycle fatigue and metallurgical properties of laser metal wire deposited Ti-6Al-4V
Luleå University of Technology, Department of Engineering Sciences and Mathematics, Material Science.ORCID iD: 0000-0001-5921-1935
Luleå University of Technology, Department of Engineering Sciences and Mathematics, Material Science.ORCID iD: 0000-0002-7675-7152
Luleå University of Technology, Department of Engineering Sciences and Mathematics, Material Science.ORCID iD: 0000-0003-3661-9262
2016 (English)In: International Journal of Fatigue, ISSN 0142-1123, E-ISSN 1879-3452, Vol. 87, p. 245-256Article in journal (Refereed) Published
Abstract [en]

Additive manufacturing (AM) has achieved large attention within the aerospace industry mainly because of the possibility to lower the material and the manufacturing cost. For titanium alloys several AM techniques are available today. In the present paper, the focus has been on laser metal wire-deposition of Ti-6Al-4V. Walls were built and low cycle fatigue specimens were cut out in two orientations with respect to the deposition direction. An extensive fractographic evaluation was carried out after testing and the results indicated anisotropic behaviour at low strain ranges. Defects such as pores and lack of fusion (LoF) were observed and related to the fatigue life and specimen orientation. The LoF defects are regarded to have the most detrimental influence on the fatigue life, whilst the effect of pores was not as straightforward. Noteworthy in present study is that one large LoF defect did not influence the fatigue life, which is explained by the prevalence of the LoF defect in relation to the loading direction.

Place, publisher, year, edition, pages
2016. Vol. 87, p. 245-256
National Category
Other Materials Engineering
Research subject
Engineering Materials
Identifiers
URN: urn:nbn:se:ltu:diva-5610DOI: 10.1016/j.ijfatigue.2016.02.011ISI: 000374615900026Scopus ID: 2-s2.0-84958951831Local ID: 3c23bc11-ab50-4499-8cb0-c65a627389a7OAI: oai:DiVA.org:ltu-5610DiVA, id: diva2:978484
Note
Validerad; 2016; Nivå 2; 20160215 (andbra)Available from: 2016-09-29 Created: 2016-09-29 Last updated: 2018-07-10Bibliographically approved

Open Access in DiVA

No full text in DiVA

Other links

Publisher's full textScopus

Authority records BETA

Åkerfeldt, PiaPederson, RobertAntti, Marta-Lena

Search in DiVA

By author/editor
Åkerfeldt, PiaPederson, RobertAntti, Marta-Lena
By organisation
Material Science
In the same journal
International Journal of Fatigue
Other Materials Engineering

Search outside of DiVA

GoogleGoogle Scholar

doi
urn-nbn

Altmetric score

doi
urn-nbn
Total: 404 hits
CiteExportLink to record
Permanent link

Direct link
Cite
Citation style
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Other style
More styles
Language
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Other locale
More languages
Output format
  • html
  • text
  • asciidoc
  • rtf