Quantifying Hydrogen Concentrations and their Influence on Surface-Initiated Damage in Rolling/Sliding Contacts of 100 Cr6 Bearing Steel
Luleå University of Technology, Department of Engineering Sciences and Mathematics, Machine Elements.ORCID iD: 0000-0003-1961-2632
Luleå University of Technology, Department of Engineering Sciences and Mathematics, Machine Elements.
Department of Materials Development, Corrosion and Hydrogen Embrittlement Group, Swerim AB, Lulea, Sweden.
Luleå University of Technology, Department of Engineering Sciences and Mathematics, Machine Elements.ORCID iD: 0000-0003-3123-0303
Show others and affiliations
2025 (English)In: Tribology letters, ISSN 1023-8883, E-ISSN 1573-2711, Vol. 73, article id 73Article in journal (Refereed) Published
Abstract [en]

This work investigates the quantitative effect of the hydrogen concentration of 100Cr6 bearing steel on the surface-initiated damage induced during lubricated rolling/sliding tribotesting. Hydrogen was introduced to the samples prior to tribotesting by electrochemical pre-charging, and hydrogen concentration was measured using thermal desorption analysis. The surface-initiated damage was quantified by optical profilometry and scanning electron microscopy. An upper limit for the critical hydrogen concentration was determined to be 1.4–2 wppm diffusible hydrogen. At this concentration, the area fraction covered by damage features was found to double compared to uncharged samples. As both charged and uncharged samples exhibited the same type of surface damage (early-stage micropitting), it was concluded that hydrogen did not change the wear mechanism but decreased the number of contact cycles necessary for the initiation of surface defects.

Place, publisher, year, edition, pages
Springer Nature, 2025. Vol. 73, article id 73
Keywords [en]
Hydrogen embrittlement, Rolling element bearings, Micropitting, Thermal desorption analysis, Critical hydrogen concentration
National Category
Other Mechanical Engineering
Research subject
Machine Elements; Engineering Materials
Identifiers
URN: urn:nbn:se:ltu:diva-112689DOI: 10.1007/s11249-025-02004-0ISI: 001487347600002Scopus ID: 2-s2.0-105005028071OAI: oai:DiVA.org:ltu-112689DiVA, id: diva2:1958985
Funder
Luleå University of Technology
Note

Validerad;2025;Nivå 2;2025-05-19 (u5);

Full text license: CC BY 4.0;

Available from: 2025-05-19 Created: 2025-05-19 Last updated: 2026-01-28Bibliographically approved
In thesis
1. Hydrogen Embrittlement in Rolling Element Bearings
Open this publication in new window or tab >>Hydrogen Embrittlement in Rolling Element Bearings
2026 (English)Doctoral thesis, comprehensive summary (Other academic)
Abstract [en]

With the global increase of hydrogen applications and industries comes an increase in the demands for the hydrogen infrastructure, where reliability is essential. Compressors are an important part of the hydrogen infrastructure, with rolling element bearings being a key component. However, hydrogen is known to significantly reduce the mechanical properties of rolling element bearings, a phenomenon called hydrogen embrittlement. Studies report that bearings which are subjected to hydrogen can fail up to ten times faster compared to bearings operating in other conditions. This detrimental effect on bearing performance has led to research within the subject of hydrogen embrittlement in bearing steels. While it is well established in research that hydrogen affects bearings negatively, several research challenges remain. This includes both the fundamental level to further understand the interaction of hydrogen with the steel as well on a more applied level when it comes to the quantification of hydrogen damage, as most of the research available in hydrogen embrittlement has a qualitative character. 

In this research, rolling sliding tribotesting using a micropitting rig (MPR) as well as full bearing testing were performed to further understand the interaction between hydrogen and bearing steel. These tribotests were combined with electrochemical hydrogen charging, thermal desorption mass spectrometry (TDMS) as well as extended material analysis to connect the wear to the hydrogen concentration as well as hydrogen trapping state in the bearing steel. The hydrogen trapping state in the material is of importance, as a lower hydrogen trapping energy is often correlated with a higher potential of hydrogen embrittlement. The results have shown that the cyclic straining of bearing steel during tribotesting can lower the hydrogen trapping energy, highlighting the increased embrittling effect of hydrogen in bearing applications. Another finding was a quantitative correlation between diffusible hydrogen concentration of bearing steel and surface-initiated damage. The hydrogen concentration of bearing steel was systematically varied by different hydrogen pre-charging conditions, which was then followed by tribotesting and wear quantification. Results revealed that at a hydrogen concentration between 1.4-2 wppm, the wear quantity doubled, while the wear mechanisms remained the same. A novel in situ hydrogen charging full thrust bearing test rig, the Hydrogen Embrittlement in Rolling Element Bearings (HERo) rig, has been developed. This test rig offers several advantages compared to test setups previously described in the literature. As a result of in situ charging, the diffusible hydrogen concentration during tribotesting is not decreasing as in conventional setups where pre-charging is performed prior to tribotesting. This allows for a more precise measurement of the influence of hydrogen on bearing steel. Furthermore, the charging in the HERo rig is performed via the backside of the bearing washer, meaning that the electrolyte is never in contact with the wear track, preventing corrosion or alteration of the surface roughness. The experiments performed with the HERo test rig show a significant decrease in bearing runtime under the influence of hydrogen by a factor of 3. While tests without hydrogen charging failed due to lubricant degradation and surface-initiated wear, hydrogen charged tests failed due to sub-surface initiated macropitting with the presence of white etching cracks. When varying hydrogen pre-charging and in situ charging procedures, it was found that longer pre-charging led to earlier bearing fatigue, while the damage mechanism stayed identical for the different hydrogen concentrations. This indicates that a critical hydrogen concentration exists not only for surface-initiated wear as mentioned above, but also for the initiation of sub-surface crack networks and macropitting. Lastly, it was found that hydrogen promoted not only the formation of white etching cracks and white etching areas, but also martensitic decay and formation of dark etching areas. 

In summary, results of the project confirm the detrimental effect of hydrogen on bearing steel, and add quantitative data to the state of knowledge, making it possible to industrially use the research data for more reliable bearings in hydrogen environments. 

Place, publisher, year, edition, pages
Luleå: Luleå University of Technology, 2026
Series
Doctoral thesis / Luleå University of Technology, ISSN 1402-1544
Keywords
Rolling Element Bearing, Hydrogen Embrittlement, Tribology, Fatigue, Test rig design
National Category
Other Mechanical Engineering
Research subject
Machine Elements
Identifiers
urn:nbn:se:ltu:diva-116224 (URN)978-91-8048-981-2 (ISBN)978-91-8048-982-9 (ISBN)
Public defence
2026-03-26, E231, Luleå University of Technology, Luleå, 09:00 (English)
Opponent
Supervisors
Available from: 2026-01-29 Created: 2026-01-28 Last updated: 2026-03-05Bibliographically approved

Open Access in DiVA

fulltext(4821 kB)104 downloads
File information
File name FULLTEXT01.pdfFile size 4821 kBChecksum SHA-512
0b80141062c60ef3b2cf7e68be59ddc8f83b552fb3021252a8aeb74c5fee6a96bf45d5b835ac96469148b82163490e93b85953ebb4df5bfb26f4c19641ebc9c5
Type fulltextMimetype application/pdf

Other links

Publisher's full textScopus

Authority records

Weniger, Lisa-MariePelcastre, LeonardoÅkerfeldt, PiaHardell, Jens

Search in DiVA

By author/editor
Weniger, Lisa-MarieJamil, KinzaPelcastre, LeonardoÅkerfeldt, PiaHardell, Jens
By organisation
Machine ElementsMaterial Science
In the same journal
Tribology letters
Other Mechanical Engineering

Search outside of DiVA

GoogleGoogle Scholar
Total: 106 downloads
The number of downloads is the sum of all downloads of full texts. It may include eg previous versions that are now no longer available

doi
urn-nbn

Altmetric score

doi
urn-nbn
Total: 533 hits
CiteExportLink to record
Permanent link

Direct link
Cite
Citation style
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Other style
More styles
Language
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Other locale
More languages
Output format
  • html
  • text
  • asciidoc
  • rtf